THE SCIENCE OF SIMULATION / MATERIAL RESPONSE

Stretch it.
Question the curve.

Pull a virtual elastomer. Watch its shape change, then connect deformation to force.

Your first experiment

Run the tensile test. Watch the specimen stretch and its cross-section shrink. Why can nominal stress and true stress be different while describing the same force?

VIRTUAL MATERIAL TEST

Make the material respond.

Target state preview

Ideal uniform gauge section. Grid lines are material markers, not a finite element solution.

Initial length L₀ = 50 mm.
Initial square section A₀ = 100 mm².

Sliders instantly preview the target state. Run sweeps from λ = 1 to that target; animation speed has no material-rate meaning.

Current λ = 1.60
Target λ = 1.60
True stress σPendingforce / current area
Nominal stress PPendingforce / original area
Tensile force FPendingsame force, either stress measure
Initial Young’s modulus E₀Pendingsmall-strain slope = 3μ

Follow the point. Read the axes.

Both curves describe the same constitutive law.

Try another experiment · double the stiffness

Same deformation. Twice the stiffness.

Keep λ fixed and double μ. This model predicts exactly twice the stress and force, while the geometry remains unchanged. Pin your current material, change μ, then compare both curves.

No comparison pinned.

What should not change?

With displacement controlled, both materials have the same length and cross-section. A different force is needed to hold the same stretch. A force-controlled test would ask a different question and would solve for λ instead.

Try the comparison and inspect the violet baseline on the graph.

Understand the model · from deformation to stress

The stretch ratio λ = L/L₀ describes the deformation you impose. The shear modulus μ describes the material’s stiffness. Increasing λ changes the shape. Increasing μ at the same λ changes the force required to hold that shape.

This ideal specimen is incompressible: its length increases while both lateral dimensions decrease. There is no damage, permanent set or time dependence in this model.

From stored energy to stress.

A hyperelastic material stores energy as it deforms. For this incompressible neo-Hookean model, the uniaxial deformation gives:

W = ½ μ(λ² + 2/λ − 3)
P = dW/dλ = μ(λ − λ⁻²)
σ = λP = μ(λ² − λ⁻¹)

W is energy per initial volume. P is nominal stress. σ is true, or Cauchy, stress. Both stress measures are in MPa, equivalent to N/mm².

The geometry keeps the accounting honest.

λ₁ = λ; λ₂ = λ₃ = λ⁻½
J = λ₁λ₂λ₃ = 1
A = A₀/λ; F = PA₀ = σA

The volume ratio J stays at one. A narrower current cross-section means the same tensile force produces a larger true stress than nominal stress. At λ = 1, both stresses vanish.

Near λ = 1, the tangent is E₀ = 3μ. At larger strains, neither the stress nor the geometry should be extrapolated from a single small-strain straight line.

Assumptions and sources

This is a homogeneous uniaxial, incompressible, isotropic neo-Hookean constitutive calculation. It evaluates closed-form equations; it does not solve a spatial finite element mesh. The visible grid tracks material points, and colour is uniform because this ideal gauge section has uniform axial stress.

The model ignores gripper constraints, local necking, rupture, damage, hysteresis, rate dependence and temperature. Its parameter values are illustrative. The curve is generated from a law, not experimental measurements; no real material is certified by this demonstration. A real material model needs calibration and checks against independent test modes.

The uniaxial reduction, plots and interactive implementation are independently derived for this educational experiment.

Take this into FEM: a material law turns deformation into stress. A finite element model connects those local responses into the behaviour of a structure.